Chemical analysis

AISI: 321
W.N.: 1.4878
C max: 0.01
Si max: 1.00
Mn max: 2.00
P max: 0.045
S max: 0.015
Cr: 17-19
Ni: 9-12

Characteristics and areas of application

1.4878 heat-resistant austenitic stainless steel is used for construction applications while the maximum temperature resistance reaches up to 850°C. It can also be customized due to the effect of a sulfur gas environment.