1.4845/310S

Chemical analysis

AISI: 310S
W.N.: 1.4845
C max: 0.10
Si max: 1.50
Mn max: 2.00
P max: 0.045
S max: 0.015
Cr: 24-26
Ni: 19-22
N max: 0.10

Characteristics and areas of application
Heat-resistant austenitic stainless steel. It is used to make parts for furnaces, heat exchangers, burners, endothermic engines and equipment for the chemical and petroleum industries.