Materials Austenitic steel
1.4570/303Kx
Chemical analysis
AISI: 303Kx
W.N.: 1.4570
C max: 0.08
Si max: 1.00
Mn max: 2.00
P max: 0.045
S max: 0.15-0.35
Cr: 17-19
Ni: 8-10
N max: 0.10
Cu max: 1.40-1.80
Mo max: 0.60
Characteristics and areas of application
Austenitic Cr-Ni stainless steel. It possesses mechanical properties similar to those of 1.4305 but the addition of Cu improves its corrosion resistance and processing features in chip removal machinery.