Materials Austenitic steel
1.4310/302
Chemical analysis
AISI: 302
W.N.: 1.4310
C : 0.05-0.15
Si max: 2.00
Mn max: 2.00
P max: 0.045
S max: 0.015
Cr: 16-19
Ni: 6-9.5
Characteristics and areas of application
Austenitic grade of stainless steel with higher carbon compared to 1.4307. 1.4310 is used in the manufacturing of fittings, flanges, bolts, valves, pump and compressor shafts, dies, cables and many other products. In addition, this austenitic grade is used specifically and extensively in the manufacture of springs and where greater strength is required after cold deformation process.